As a starting materials of ceramics, various synthetic whitlockite solid solutions ((Mg,Fe)-CaW) replaced with Fe2+ ion at Mg site in the whitlockite were _successfully prepared by wet chemical method. The whitlockite compact sintered above 900°C in air. The sinterability of the compacts and bending strength of whitlockite ceramics increased with firing temperature, and fell with increasing of Fe2+ ion content. The maximum three bending strength of whitlockite ceramics reached at about 75 MPa when the (Mg0.7,Fe0.3)-CaW compact was heated at 1000°C for 24 h.