Naohiro Hayashi,Ken Watanabe
标识
DOI:10.1002/advs.202512219
摘要
Abstract Co‐sintering cathode materials with Li 7 La 3 Zr 2 O 12 (LLZ) is a promising strategy for fabricating bulk‐type all‐solid‐state batteries (ASSBs). However, preventing reactions between different materials, which is difficult with high‐capacity cathode materials such as LiNi 0.6 Mn 0.2 Co 0.2 O 2 (NMC622), is a pre‐requisite for applying this strategy. To overcome this issue, Li 1+ x Ni 0.6 Mn 0.2 Co 0.2 O 2 ( x = 0.01–0.2), which intentionally deviates from the stoichiometric NMC622 composition, is synthesized here. The formation of impurity phases in the co‐sintering process can be controlled by adjusting the co‐sintering temperature and x . Impurity phases are not formed on co‐sintering with x = 0.075 at 800 °C because reduced cation mixing in NMC622 and the presence of a self‐formed Li 2 CO 3 layer on the particle surface, ensured by adjusting x , effectively suppresses reactions. Furthermore, good results are observed at sintering temperatures where the proportions of Ni 2+ and Co 2+ , which promote cation mixing, are low. This study clarifies relevant reaction mechanisms using various analytical methods (such as temperature‐rise X‐ray absorption fine structure analysis and scanning transmission electron microscopy‐electron energy loss spectroscopy), and confirms the repetitive operation of bulk‐type ASSBs assembled using co‐sintered Li 1+ x Ni 0.6 Mn 0.2 Co 0.2 O 2 ( x = 0.075)/LLZ electrolyte systems. The method reported herein can be potentially adopted for cost‐effective and high‐energy‐capacity ASSB production.
科研通智能强力驱动
Strongly Powered by AbleSci AI