材料科学
复合材料
环氧树脂
失效模式及影响分析
断裂韧性
韧性
胶粘剂
剪切(地质)
镁
断裂(地质)
冶金
图层(电子)
作者
Yingcai Pan,Guoqing Wu,Xu Cheng,Zongke Zhang,Maoyuan Li,Sudong Ji,Zheng Huang
标识
DOI:10.1080/09276440.2016.1144911
摘要
The fiber metal laminates (FML), consisting of carbon fiber reinforced polymer prepregs and magnesium alloys sheets, were introduced, and the Mode I (peel) and Mode II (shear) interlaminar fracture toughness of the FMLs were investigated. The results show that the Mode I interlaminar toughness (0.23 kJ/m2) of the FMLs is much lower than the Mode II interlaminar toughness (5.81 kJ/m2), due to the fact that the effects of mechanical interlock to hinder crack propagates is smaller under Mode I loading conditions than under Mode II. The FMLs mainly show adhesive failure and interfacial failure under Mode I loading conditions, while for Mode II loading, it exhibits a degree of epoxy cohesive failure except the adhesive failure and interfacial failure.
科研通智能强力驱动
Strongly Powered by AbleSci AI