摘要
Abstract Supercritical carbon dioxide readily induces crystallization in bisphenol A polycarbonate. Crystallization begins within one h of exposure to the CO2 at temperatures and pressures as low as 75°C and 100 atm. The degree of crystallinity increases sharply as the CO2 pressure is raised from 100 to 300 atm but levels off thereafter. This behavior is likely due to a minimum in the Tg of the polycarbonate/CO2 mixture owing to the opposite effects of the pressure on the Tg of the polymer and on the equilibrium weight fraction of CO2 absorbed. Percent crystallinities of over 20%, comparable to that achieved using acetone or other organic liquids, have been obtained after 2 h exposure to supercritical CO2. Since polycarbonate degasses quickly and quantitatively at ambient temperature and pressure, the high Tg of bisphenol A polycarbonate can be regained in the crystallized material without further vacuum treatment.
科研通智能强力驱动
Strongly Powered by AbleSci AI