摘要
Morphological instability of the lithium-electrolyte interface is a critical problem limiting the development of lithium-metal anodes for both liquid and solid-state cells. In liquid cells, unstable deposition produces filaments (or "dendrites") and dense arrays of filaments termed "moss" (1,2). Significant stabilization of the interface is achieved by use of ether-based electrolytes and applied stack pressure in the range 0.1-0.3 MPa (3, 4). Microscopic studies reveal that filaments grow by addition of Li atoms at their base (5,6), as a result of diffusion of plated Li atoms into the anode (7). Previously, we characterized diffusion by modeling in situ measurements of stress evolution (8) and Li diffusion in the current collector (9). It was found that in both experiments, on the order of 1 % of the plated Li atoms diffused into the anode (10-12). We present an integrated model of anode morphology evolution that includes effects of stack pressure and electrolyte chemistry. The model incorporates diffusion in the anode accommodated by power-law creep, and ion conduction in the electrolyte. The anode-polymer separator interface is microscopically rough, permitting Li creep in response to pressure gradients. Electrolyte chemistry affects morphology through Li surface energy (12). Interface evolution is tracked by linear stability analysis; that is, small periodic disturbances are applied at the interface, and the growth rate of the disturbance amplitude is predicted. Diffusion and creep parameters are taken from literature sources (13,14). Calculations demonstrate that during plating at 1 mA/cm 2 , the anode interface is unstable at stack pressure below 0.1 MPa, but stable at pressure above 0.5 MPa. This range is similar to the critical range of stack pressures found in experiments (4). Stabilization is due to creep away from incipient peaks on the Li interface. Similar creep-induced stabilization is found at increased surface energies, as are thought to characterize ether-based electrolytes (3). Increased anode thickness also induces stabilization by reducing the flow resistance for creep away from Li peaks. Overall, the model provides an integrated quantitative framework to rationalize chemical and mechanical influences on Li anode stability. REFERENCES P. Bai, J. Li, F. R. Brushett, M. Z. Bazant, Energy Environ. Sci., 9, 3221 (2016). L Frenck, G. K. Sethi, J. A. Maslyn, N. P. Balsara, Front. Energy Res., 7, 115 (2016) D. T. Boyle et al. J. Amer. Chem. Soc., 144, 20717 (2022). C. C. Fang et al., Nat. Energy, 6 987 (2021). A. Kushima, et al., Nano Energy, 32, 271 (2017). J. Becherer, D. Kramer, R. Moenig, J. Mater. Chem. A, 10, 5530 (2022). X. Wang, et al., Nat. Energy, 3, 227 (2018). J. H. Cho et al., Energy Storage Mater., 24, 281 (2020). S. Lv et al., Nat. Comms., 9, 2152 (2018). K. R. Hebert, J. Electrochem. Soc., 170, 110537 (2023) K. R. Hebert, J. Power Sources 617, 235098 (2024). K. R. Hebert, submitted (2025). T. Krauskopf, Chem. Rev. 120, 7745 (2020). S. Naryan and L. Anand, Extreme Mech. Lett., 24, 21 (2018).