摘要
The role of catalyst stability on the adverse effects of hydrogen peroxide (H 2 O 2 ) formation rates in a proton exchange membrane fuel cell (PEMFC) is investigated for Pt, Pt binary (PtX, X = Co, Ru, Rh, V, Ni) and ternary (PtCoX, X = Ir, Rh) catalysts supported on ketjen black (KB) carbon. The selectivity of these catalysts towards H 2 O 2 formation in the oxygen reduction reaction (ORR) was measured on a rotating ring disc electrode. These measured values were used in conjunction with local oxygen and proton concentrations to estimate local H 2 O 2 formation rates in a PEMFC anode and cathode. The effect of H 2 O 2 formation rates on the most active and durable of these catalysts (PtCo and PtIrCo) on Nafion membrane durability was studied using a single-sided membrane electrode assembly (MEA) with a built-in reference electrode. Fluoride ion concentration in the effluent water was used as an indicator of the membrane degradation rate. PtIrCo had the least fluorine emission rate (FER) followed by PtCo/KB and Pt/KB. Though PtCo and PtIrCo show higher selectivity for H 2 O 2 formation than unalloyed Pt, they did not contribute to membrane degradation. This result is explained in terms of catalyst stability as measured in potential cycling tests in liquid electrolyte as well as in a functional PEM fuel cell.
科研通智能强力驱动
Strongly Powered by AbleSci AI