High Resolution Image Download MS PowerPoint Slide Cube- and tube-shaped C 70 crystals were obtained selectively by reprecipitation using a combination of mesitylene (good solvent) and isopropyl alcohol (poor solvent). Both crystals include mesitylene molecules in their lattices; the ratios of C 70 to mesitylene were 1:2 in C 70 cubes and 1:0.7 in C 70 tubes. The volume ratio of mesitylene to IPA is a key parameter for the selective growth of C 70 cubes and C 70 tubes, rather than the supersaturation ratio, which governs crystal morphology in many other cases. Thus, we propose that the absolute amount of mesitylene near C 70 molecules determines the crystallization pathways for forming the C 70 ·2(mesitylene) or C 70 ·0.7(mesitylene) phase, which finally result in C 70 cubes or C 70 tubes, respectively.