Xi Zhang,Kaijing Niu,Weixiao Song,Shouke Yan,Xiuying Zhao,Yonglai Lu,Liqun Zhang
标识
DOI:10.1002/marc.201900042
摘要
The effect of epoxidation on strain-induced crystallization (SIC) of epoxidized natural rubber (ENR) and mechanism are studied with synchrotron radiation wide-angle X-ray diffraction (SR-WAXD) and polarized infrared spectroscopy (P-IR). WAXD results reveal that appropriate epoxidation, for example, ENR-25 epoxidized with ≈25% isoprene units, can unexpectedly enhance the SIC of natural rubber (NR), resulting in the improvement of tear resistance. On the other hand, exorbitant epoxidation, for example, ENR-40 epoxidized with ≈40% isoprene units, depresses the SIC and weakens the mechanical properties of NR remarkably. P-IR studies reveal that epoxidation can promote the orientation of chain segments along the stretching direction, which plays a determining role on SIC of NR. Accordingly, hierarchical multiscale schematic models are proposed. This insight into epoxidation on SIC of ENR strongly suggests that ENR with appropriate epoxidation degree is a promising candidate material for the fabrication of high-performance engineering rubber products.
科研通智能强力驱动
Strongly Powered by AbleSci AI