作者
Maude Bert,Jean-Philippe Colonna,Jacopo Celè,Lara Casiez,Sami Oukassi,Sylvain Franger
摘要
Anode-less configuration appears as promising for the future of all-solid-state batteries (SSB) with its maximal energy density. However, long-term cycling is still limited due to evolving interfacial resistance. Therefore, understanding the failure mechanisms at the negative electrode/electrolyte interface remains one of the main challenges. A key parameter for the uniformity and the nucleation of the electrodeposited layer is the current density. Links have been made with the increase of interfacial charge transfer resistance [1], [2]. Nevertheless, observations are often confined to the early stages of lithium nucleation and the subsequent evolution upon cycling remains unclear. In order to study fully charged batteries, we used a simple method to prepare samples that enable easy SEM observations. It consists in cleaving manually thin film batteries prior to charging and transferring them with an air-free holder to the SEM equipment. Batteries are made of a LiCoO2 positive electrode, a LiPON electrolyte and a Ti substrate as (negative) current collector (CC). We, first, confirmed the evolution of the lithium morphology as a function of the charging current density with SEM cross-sections (figures a-c). The higher the charging current, the more uniform the thickness of the deposited negative electrode. Contrarily to the previous studies [1], [3], we highlighted that the lithium plated between the Ti CC and the LiPON glassy electrolyte presents a specific aspect with the formation of a dense columnar layer (figure d). Secondly, the internal resistance measured by electrochemical impedance spectroscopy (figure e) seems well correlated to the variation of roughness shown on SEM-images (figures a-c). In the Nyquist plot (figure e), the second semi-circle attributed to interfacial resistance is 1.2 higher at 0.025mA.cm-2 than at 2.5mA.cm-2. Therefore, the combination of both electrical measurements and SEM cross-sections observations should make it possible to figure out what kind of physical heterogeneities or defects occur during cycling and finally decrease the efficiency of anode-less SSB after several lithium stripping and plating. References: [1] T. Fuchs et al., « Current-Dependent Lithium Metal Growth Modes in “Anode-Free” Solid-State Batteries at the Cu|LLZO Interface », Advanced Energy Materials, vol. 13, no 1, p. 2203174, 2023, doi: 10.1002/aenm.202203174. [2] F. Sagane, K. Ikeda, K. Okita, H. Sano, H. Sakaebe, et Y. Iriyama, « Effects of current densities on the lithium plating morphology at a lithium phosphorus oxynitride glass electrolyte/copper thin film interface », Journal of Power Sources, vol. 233, p. 34-42, juill. 2013, doi: 10.1016/j.jpowsour.2013.01.051. [3] D. Cheng et al., « Unveiling the Stable Nature of the Solid Electrolyte Interphase between Lithium Metal and LiPON via Cryogenic Electron Microscopy », Joule, vol. 4, no 11, p. 2484-2500, nov. 2020, doi: 10.1016/j.joule.2020.08.013. Figure 1