作者
Ruijun Zhang,Mingkun Zhang,Guangzhao Zhang,Yujian Chen,Jia Liu,Ziqian Tian,Ye Yu,Peng 鹏 Zhao 赵,Jiafa Cai,Xiaping Chen,Dingqu Lin,Shao-xiong Wu,Yuning 宇宁 Zhang 张,Xingliang Xu,Rongdun Hong,Feng Zhang
出处
期刊:Chinese Physics B
[IOP Publishing]
日期:2025-03-24
卷期号:34 (6): 067201-067201
被引量:5
标识
DOI:10.1088/1674-1056/adc407
摘要
A minority carrier lifetime of 25.46 μs in a P-type 4H-SiC epilayer has been attained through sequential thermal oxidation and hydrogen annealing. Thermal oxidation can enhance the minority carrier lifetime in the 4H-SiC epilayer by reducing carbon vacancies. However, this process also generates carbon clusters with limited diffusivity and contributes to the enlargement of surface pits on the 4H-SiC. High-temperature hydrogen annealing effectively reduces stacking fault and dislocation density. Moreover, electron spin resonance analysis indicates a significant reduction in carbon vacancy defects after hydrogen annealing. The mechanisms of the elimination of carbon vacancies by hydrogen annealing include the decomposition of carbon clusters formed during thermal oxidation and the low-pressure selective etching by hydrogen, which increases the carbon content on the 4H-SiC surface and facilitates carbon diffusion. Consequently, the combination of thermal oxidation and hydrogen annealing eliminates carbon vacancies more effectively, substantially enhancing the minority carrier lifetime in P-type 4H-SiC. This improvement is advantageous for the application of high-voltage SiC bipolar devices.
科研通智能强力驱动
Strongly Powered by AbleSci AI