Abstract Thin films of HfO2 are deposited by liquid injection metal‐organic (MO) CVD and atomic layer deposition (ALD) using the new cyclopentadienyl precursors [(MeCp)2HfMe(OiPr)] and [(MeCp)2HfMe(mmp)] (mmp = OCMe2CH2OMe). Both precursors evaporate at moderate temperatures, making them very suitable for MOCVD and ALD applications. Thin films of HfO2 are deposited by MOCVD in the temperature range 400–650 °C, and by ALD in the temperature range 300–450 °C, using both [(MeCp)2HfMe(OiPr)] and [(MeCp)2HfMe(mmp)] . Analysis by X‐ray diffraction (XRD) shows that the films are deposited with an essentially amorphous microstructure, but subsequent annealing above 700 °C in dry air crystallizes the films into the α‐ or monoclinic phase. Auger electron spectroscopy (AES) shows that residual carbon (0–5 at.‐ %) is present in the oxide films and that the HfO2 films grown by MOCVD generally contain more carbon than those grown by ALD. The dielectric properties of the as‐deposited HfO2 films are evaluated using [Al/HfO2/SiO2/n‐Si] MOS capacitor structures with various HfO2 thicknesses ranging from 1.7 nm to 102 nm. The calculated permittivity (ϵox), assuming the presence of a 1 nm native SiO2 interlayer, is found to be ϵox ∼ 14 for a HfO2 film grown by ALD using [(MeCp)2HfMe(OiPr)], whilst for a film grown by ALD using [(MeCp)2HfMe(mmp)], ϵox is found to be ∼10. Equivalent oxide thicknesses of 2.5 and 0.78 nm are measured for HfO2 films deposited by ALD using [(MeCp)2HfMe(OiPr)] and [(MeCp)2HfMe(mmp)], respectively. The leakage current density for a film grown by ALD using [(MeCp)2HfMe(OiPr)] remains very low (<10–6 A cm–2) up to 2.5 MV cm–1, whereas the leakage current density is significantly higher for the MOCVD‐grown films.