PEG比率
杰纳斯
化学工程
材料科学
化学
纳米技术
财务
工程类
经济
作者
Jiacong Wu,Shiyuan Liu,Xinnan Ma,Cailiang Zhang,Chengxiang Feng,Lei Wang,Juan Han,Yun Wang
出处
期刊:Langmuir
[American Chemical Society]
日期:2024-01-09
卷期号:40 (3): 1774-1784
被引量:2
标识
DOI:10.1021/acs.langmuir.3c03026
摘要
The current study presents a scalable approach for the preparation of temperature-responsive PEG/SiO2/PNIPAM-PEA Janus particles and, for the first time, investigates their potential applications in stabilizing foam and defoaming by adjusting the temperature. The method utilizes a (W1 + O)/W2 emulsion system, which incorporates appropriate surfactants to stabilize the emulsion and prevent rapid dissolution of the hydrophilic triblock polymer PEG-b-PTEPM-b-PNIPAM in water. The PEG/SiO2/PNIPAM-PEA Janus particles with temperature-responsive characteristics were synthesized in a single step that combined the sol–gel reaction and photoinduced free radical polymerization. The contact angle of the hydrophilic PEG/SiO2/PNIPAM surface was measured to be 54.7 ± 0.1°, while the contact angle of the hydrophobic PEA surface was found to be 122.4 ± 0.1°. By incorporating PEG/SiO2/PNIPAM-PEA Janus particles at a temperature of 25 °C, the foam’s half-life is significantly prolonged from 42 s to nearly 30 min. However, with an increase in temperature to 50 °C, the foam’s half-life rapidly diminished to only 44 s. This innovative application effectively enhances foam stabilization at low temperatures and facilitates the rapid dissipation of foam at high temperatures.
科研通智能强力驱动
Strongly Powered by AbleSci AI