Rusong Chen,Chunxia Yao,Qi Yang,Hongyi Pan,Xiqian Yu,Kai Zhang,Hong Li
标识
DOI:10.1021/acsami.1c01246
摘要
All-solid-state batteries (ASSBs) are expected to address the battery safety issues fundamentally by replacing the flammable electrolyte with solid electrolytes (SEs). However, recent studies report that the thermal runaway happened for NASICON-type SEs when they contact with Li metal at high temperature and indicate that the ASSBs may not be totally safe. Here, the thermal stability of a NASICON-type Li 1.4 Al 0.4 Ti 1.6 (PO 4 ) 3 (LATP) SE pellet against metallic lithium is quantified in a quasi-practical situation. Accelerated thermal runaway of the LATP pellet compared to LATP powder is observed when they contact with lithium. Combining electrochemical impedance spectroscopy and X-ray computed tomography analysis, lithium penetration into the pellet at high temperature has been observed. The penetrated lithium without surface impurities and the high reactivity of LATP at defect sites (atomic structural defects, cracks, voids, etc.) lead to higher interfacial reactivity and earlier thermal runaway. By adding LiPO 2 F 2 to modify those defect sites of the LATP pellet and impede the lithium/SE interfacial reactions, the thermal runaway can be remarkably delayed. This work elucidates the thermal runaway behaviors of Li/LATP pellets in a quasi-practical environment, provides new information about safety issues of ASSBs, and inspires future investigations into this urgent-needed area.
科研通智能强力驱动
Strongly Powered by AbleSci AI