摘要
A new violet phosphor was synthesized by sintering under the reduction condition from the Sr–Al–O:Eu powder oxidized from an ethylenediaminetetraacetic (EDTA) complex on a polycrystalline alumina plate. The crystalline phase of violet phosphor was determined to be Sr 7 Al 12 O 25 by the change in the crystallinity of the product with a change in the composition of the raw material. The emission wavelength of the phosphor was 410 nm for Sr 7 Al 12 O 25 :Eu 2+ . For the composition of Sr:Al:Eu = 6.86:8:0.14 in the EDTA complex with sintering at 1400 °C, Sr 7 Al 12 O 25 :Eu 2+ was obtained only in the crystalline phase of Sr 7 Al 12 O 25 and exhibited the highest emission intensity of 410 nm in our experiment. The sintering temperature at sintering and composition of metals in the EDTA complex affected the emission wavelength change from 410 to 460 nm because of change in crystallinity. These changes indicate that the emission color in the range from violet to green is controlled by composition change or sintering temperature.
科研通智能强力驱动
Strongly Powered by AbleSci AI