Sujit Suresh Oswal,Purvaja Salil Nene,Pallavi B Madanshetty,Ramandeep Dugal
出处
期刊:Universal Research Journal of Dentistry
日期:2016-01-01
卷期号:6 (2): 190-190
标识
DOI:10.4103/2249-9725.181697
摘要
The optical behavior of the final restoration is determined by the color of the underlying tooth structure, the color of the luting agent, and the thickness and opacity of the ceramic material used. This article reports a case in which veneers and full crowns made of heat-pressed, lithium disilicate glass-ceramic were used for the esthetic rehabilitation of anterior discolored teeth. The patient was referred for treatment with defective anterior composite resin restorations, darkening of the gingival margins, and uneven gingival contours. The multidisciplinary treatment plan included dental bleaching, periodontal plastic surgery to create gingival symmetry, and indirect all-ceramic restorations using translucency lithium disilicate glass-ceramic ingots to achieve an excellent esthetic result.
科研通智能强力驱动
Strongly Powered by AbleSci AI