摘要
Zeolites have attracted significant attention in the fields of catalysis, adsorption, and separation due to their well-defined pore architecture, high thermal stability, and tunable acidity. Various zeolites have proven to be highly versatile, offering a unique combination of microporosity, catalytic activity, and shape-selectivity suitable for numerous industrial applications. However, conventional hydrothermal synthesis methods, which typically rely on aqueous media and organic structure-directing agents (OSDAs), often present limitations in terms of crystal morphology control, porosity optimization, and environmental sustainability. Ionic liquids (ILs) have emerged as promising solvents and SDAs for the synthesis of zeolitic materials. Owing to their unique physicochemical properties, such as low vapor pressure, high thermal stability, and abundant ion combinations, ILs provide a versatile medium for crystal growth under milder and more controllable conditions. The application of ILs in zeolite synthesis, commonly referred to as ionic-liquid-templated or ionothermal synthesis, offers a paradigm shift in material design. In this work, both of the templating effect and ionothermal strategy were studied. The crystal growth kinetics were analyzed, and a mechanism was proposed to guide further studies on structural development, linking synthesis conditions to potential applications. In the early stage of this work, various ILs including 1,5-dibromopentane, 1-methylpyrrolidine, 1-ethyl-3-ethylimidazolium bromide, 1-Ethyl-1-methylpyrrolidinium bromide, 1-butyl-3-methylimidazolium bromide and 1-butyl-3-methylimidazolium chloride, were used to reveal the topology structure of the zeolite synthesis from different ionic liquids. Results showed that the ANA was synthesized from 1,5-dibromopentane, 1-methylpyrrolidine, 1-ethyl-3-ethylimidazolium bromide, 1-Ethyl-1-methylpyrrolidinium bromide at Si/Al ratios 20-50. While higher Si/Al ratios and extended hydrothermal treatment led to the transformation of ANA to MOR. TON and MFI were successfully prepared from imidazolium-based templates, with the pure phase of MFI formation templated by 1-butyl-3-methylimidazolium-based synthesis. This part provides the instructions for the following efficient and modifiable MFI synthesis. MFI zeolite, with the distinct three-dimensional porous network, has attracted wide interest in petrochemical processes and environmental applications. In this work, we utilized 1-butyl-3-methylimidazolium (BMIM)-based ILs for MFI-type zeolite synthesis, obtaining a highly crystallized MFI-type crystal in 18 h. To clarify the advantages of using ILs, ZSM-5 directed from the conventional template, tetrapropylammonium hydroxide, was prepared as a comparison. Parameters including ion variations, aging duration, and aluminate content on crystal phase growth were explored. Furthermore, seed-assisted synthesis was carried out to verify the impact of the IL on the nucleation step. The mechanism of the fast crystallization process was then revealed to show that the presence of BMIM in the synthesis gel contributed to rapid nucleation, followed by a direct formation of amorphous particles. These amorphous particles then underwent inward growth, ultimately resulting in the formation of well-crystallized particles. This finding indicates the promising potential of ILs for efficient zeolite synthesis. The ionothermal synthesis of MFI-type zeolites using [BMIM]Br, with a focus on framework development, and functional performance was also explored. By tuning synthesis parameters of temperature, Si/Al ratio, and employing a two-step heating strategy, well-crystallized ZSM-5 materials with enhanced porosity were obtained. Structural characterization by XRD, SEM, and N₂ physisorption confirmed that the two-step synthesis improved crystallinity and microporosity, while also promoting uniform mesopore formation and better pore accessibility. Functional assessments, including room-temperature N₂ adsorption, methylene blue adsorption, and catalytic toluene methylation, were conducted. Using the two-step heating treatment, the N₂ adsorption capacity of ionothermally synthesized zeolites increased from 2.57 cm3/g to 3.86 cm3/g, and methylene blue adsorption (within 6 h) improved from 61.18 mg/kg to 74.54 mg/kg. Furthermore, toluene conversion rose by 11%, and xylene selectivity increased by 10%, confirming the enhanced structural properties achieved through the two-step heating treatment. Kinetic modeling indicated a shift from diffusion-limited physisorption in single-step samples to chemisorption-driven processes in two-step products. The recyclability of [BMIM]Br was demonstrated after single-step use, but structural degradation occurred following reuse from high-temperature treatments. Comparisons with TPAOH-templated hydrothermal syntheses further highlighted the superior structural direction offered by ILs. These findings advance the understanding of crystal growth in ionothermal systems and emphasize the potential of ILs in tailoring high-performance zeolite materials for catalytic and adsorption applications.