线性低密度聚乙烯
锥形量热计
乙烯-醋酸乙烯酯
聚乙烯
材料科学
金属
耐久性
金属氢氧化物
氢氧化物
傅里叶变换红外光谱
阻燃剂
醋酸乙烯酯
聚对苯二甲酸乙二醇酯
化学工程
复合材料
聚合物
共聚物
冶金
烧焦
工程类
热解
作者
Yi Lun Tan,Volker Wachtendorf,Tobias Kukofka,Patrick Klack,Jörg Ruder,Xuebao Lin,Bernhard Schartel
摘要
The durability of flame retardancy is a challenge for cables over long lifetimes. The degradation of flame retardance is investigated in two kinds of exposures, artificial weathering and humidity. In this basic study, typical mineral flame retardants in two polymers frequently used in cable jackets are investigated to get the fundamental picture. Aluminum hydroxide (ATH) and magnesium hydroxide (MDH) are compared in ethylene‐vinyl acetate (EVA), and further in EVA and linear low‐density polyethylene (LLDPE) cables containing the same ATH. The changes in chemical structure at the surface are studied through attenuated total reflectance Fourier transform infrared spectroscopy (ATR‐FTIR), the formation of cracks, and changes in color are investigated. The cone calorimeter and a bench scale fire testing cable module are utilized to evaluate the fire behavior of the cables. Although the flame retardancy deteriorated slightly, it survived harsh exposure conditions for 2000 h. Compared to EVA/MDH and LLDPE/ATH, the fire behavior of EVA/ATH is the least sensitive. Taken together, all of the results converge to estimate that there will be no problem with flame retardancy performance, for materials subjected to natural exposure for several years; the durability of fire retardancy is questionable for longer periods, and thus requires further investigation.
科研通智能强力驱动
Strongly Powered by AbleSci AI