煤油
材料科学
焦炭
停留时间(流体动力学)
开裂
管(容器)
石油焦
冶金
复合材料
化学
工程类
有机化学
岩土工程
作者
Ning Wang,Jin Zhou,Yu Pan,Hui Wang
出处
期刊:Advanced Materials Research
[Trans Tech Publications]
日期:2013-08-30
卷期号:750-752: 1712-1717
被引量:2
标识
DOI:10.4028/www.scientific.net/amr.750-752.1712
摘要
Coking characteristics of China RP-3 under high temperature (above 650°C) and long-duration (20 minutes) conditions, especially the effects of temperature, pressure, and inner diameter of cooling channels on coking amount were experimentally investigated. Temperature of kerosene in experiments varied from 650°C to 730°C, pressure varied from 1.8MPa to 3.5MPa, and the mass flow rate was approximately 120g/min. Results showed that temperature has a significant influence on coking amount. Even a small increment of temperature induces remarkable coke formation. However, pressure and inner diameter of the tube has a relatively little effect on it. The coking amount increases as pressure and inner diameter increase, but the increasing rate is decreasing. It is considered that inner diameter mainly affects residence time. When residence time increases to some extent, coking amount begins to grow slowly even stop increasing. This is resulted from two reasons. Firstly, the cracking conversion percentage reaches an upper limit when residence time is adequately long; secondly, coke gradually covers the inner wall of the tube, leading to isolation of kerosene from the metal surface to form coking.
科研通智能强力驱动
Strongly Powered by AbleSci AI