Soo‐Hyun Kim,Jeong‐Tae Kim,Noh-Jung Kwak,Jin Woong Kim,Tae‐Sik Yoon,Hyunchul Sohn
出处
期刊:Journal of vacuum science & technology
[American Institute of Physics]
日期:2007-08-15
卷期号:25 (5): 1574-1580
被引量:11
摘要
This article presents the effects of phases of underlying nucleation layers prepared using two different reaction schemes, one is with B2H6 and WF6 and the other with SiH4 and WF6, on the properties of chemical vapor deposited (CVD)-tungsten (W) thin film. From the x-ray diffractometry and transmission electron microscopy analysis, the B2H6-based nucleation layer was found to form as a poorly crystallized metastable β-phase W while SiH4-based one as a well-crystallized equilibrium α phase. The subsequently grown CVD-W film, as deposited with α phase, has significantly larger grains and, consequently, mitigated the increase of CVD-W resistivity due to size effect as well as lower resistivity on the B2H6-based nucleation layer than on SiH4-based one. CVD-W film on the B2H6-based nucleation layer integrated on memory devices disclosed the improved electrical properties of interconnection such as lowered contact resistance at the metal line to bit line contact, lowered bit line resistance, and reduced parasitic capacitance. These improved electrical properties are explained with the enlarged grain size of CVD-W film on the B2H6-based nucleation layer compared to that on the SiH4-based one, which is determined by the nucleation and growth behaviors on each nucleation layer.
科研通智能强力驱动
Strongly Powered by AbleSci AI