The strength of hot isostatically pressed (HIPed) silicon nitride (NT-154 produced by Norton/TRW Ceramics) was investigated after cyclic loading at room temperature and elevated temperatures. Four point bend fatigue tests were conducted in load control at an R ratio of 0.1 and a frequency of 1 Hz. The accumulated fatigue damage was assessed by stopping the test after a certain number of cycles and measuring the flexure strength at room temperature in stroke control. The effects of (i) number of cycles, (ii) maximum applied stress and (iii) temperature of cyclic loading have been studied. Increasing the temperature in the range 1200 to 1400 °C had the most detrimental effect on the residual strength. The results are explained in terms of microstructural changes.