期刊:Meeting abstracts [Institute of Physics] 日期:2025-11-24卷期号:MA2025-02 (8): 3516-3516
标识
DOI:10.1149/ma2025-0283516mtgabs
摘要
Silicon-graphite (Si/C) composite anodes offer higher specific capacity than conventional graphite anodes, but their industrial implementation is challenged by slurry aging during electrode processing. In this work, hydrogen gas (H₂) formation is identified and quantified as a key aging mechanism in commercial Si/C slurries (D 50 ≈ 9 µm, CMC/SBR binder). Slurries were systematically stored at 5 °C, 25 °C, and 45 °C for up to two weeks; gas evolution was measured using a syringe-based setup and identified by mass spectrometry. Complementary analyses including rheology, zeta potential, and pH measurements, as well as optical microscopy were performed to correlate changes in slurry properties with gas formation and electrochemical performance. Our results suggest that that H₂ originates from the reaction of silicon with residual water, leading to surface oxidation, altered slurry rheology, and degradation of particle dispersion stability. Elevated temperatures accelerated these effects, while low-temperature storage suppressed them. Electrochemical testing of 40 coin full cells confirmed that aged slurries yield reduced capacity and faster degradation. These findings highlight slurry-stage chemical reactivity as a critical factor for Si/C anode performance and emphasize the need for controlled storage conditions to mitigate aging. Figure 1