Jiao Liu,Duo Sun,Junrong Yue,Jiaming Lin,Guangwen Xu
标识
DOI:10.1021/acs.iecr.5c01670
摘要
Attrition resistance is critical for catalysts in fluidized bed reactors, where combined mechanical, thermal, and chemical stresses lead to particle degradation and performance loss. This study systematically investigates how support pretreatment and promoter modification affect the attrition resistance of spherical Ni/Al2O3 catalysts. A modified jet cup test identified two distinct attrition mechanisms: bulk fracture in catalysts supported on low-temperature calcined Al2O3 (600–900 °C) and surface abrasion in those supported on high-temperature calcined Al2O3(1100–1400 °C). The optimized catalyst 10Ni/10Mg–Al-1100 exhibited the lowest attrition index (AI = 0.54), attributed to enhanced hardness and structural integrity arising from strong NiO-MgO and MgO-Al2O3 interactions. In contrast, Mn provided limited reinforcement, leading to greater attrition. These findings highlight the critical roles of particle morphology, surface features, and metal–support interactions in enhancing the mechanical stability and attrition resistance of fluidized-bed catalysts, offering valuable insights for industrial processes such as FCC, MTO, and Fischer–Tropsch synthesis.
科研通智能强力驱动
Strongly Powered by AbleSci AI