Zipei Wan,Kai Shi,Zhong-Ming Li,Lu Yang,Qinbai Yun,Likun Chen,Fuzeng Ren,Feiyu Kang,Yan-Bing He
标识
DOI:10.1016/j.jpowsour.2021.230062
摘要
The interfacial issues between garnet electrolyte and Li metal hinder the application of garnet electrolyte in solid-state Li metal batteries. Herein, a three-dimensional (3D) porous Zn layer (PZL) is magnetron sputtered on the surface of Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 (LLZTO) to construct a 3D Li–Zn alloy layer at the LLZTO/Li interface by melting Li metal into PZL. The 3D Li–Zn alloy effectively reduces the LLZTO/Li interfacial impedance from 319.8 Ω cm 2 to an extremely low value of 1.9 Ω cm 2 . Meanwhile, the 3D alloy skeleton can enhance the transport kinetics and promote uniform distribution of Li ion at interface to inhibit the growth of Li dendrites. More importantly, the volume expansion of interface between LLZO and Li metal anode is effectively suppressed due to the host role of 3D Li–Zn alloy interface. The Li/LLZTO@PZL/Li symmetrical battery achieves a high critical current density of 2 mA cm −2 for one cycle. The all-solid-state LiNi 0.5 Co 0.2 Mn 0.3 O 2 (NCM523)/LLZTO@PZL/Li battery with a high cathode loading of 4.9 mg cm −2 delivers a high specific capacity of 143.8 mAh g −1 after 170 cycles. The 3D alloy interface is significant for enhancing the interfacial stability of high capacity all-solid-state lithium metal batteries. • A 3D Li–Zn alloy layer is constructed at Li 6.4 La 3 Zr 1.4 Ta 0.6 O 12 /Li interface. • The 3D interface can reduce interfacial impedance from 319.8 to 1.9 Ω cm 2 . • The 3D interface achieves a critical current density of 2 mA cm −2 . • The 3D interface enables high-loading solid LiNi 0.5 Co 0.2 Mn 0.3 O 2 /Li battery.
科研通智能强力驱动
Strongly Powered by AbleSci AI