Kinetic study of H 2 oxidation in the preferential oxidation (PROX) of CO was implemented over a nanosize Au/CeO 2 catalyst in a temperature range 313−353 K. The Langmuir−Hinshelwood mechanism was proposed to be mainly responsible for H 2 oxidation, and CO oxidation can be accelerated by coadsorbed H at low temperatures. On the other hand, the water in the system has proved to suppress both CO and H 2 oxidation by increasing the energy bars. In situ diffuse reflectance infrared Fourier transform spectroscopy (DRIFTS) of CO adsorption on the Au surface indicates that linear CO−Au bond can be weakened in the presence of H 2; meanwhile, water can be a poison taking effects via the bonding of water and the lattice oxygen at the interface of Au/CeO 2 . The irreversible loss of activity during reaction may be caused by the reconstruction of Au particles, at least in part.