金属有机气相外延
铟
材料科学
量子阱
光电子学
方向(向量空间)
磷化铟
外延
砷化镓
纳米技术
光学
物理
几何学
激光器
数学
图层(电子)
作者
Arne Knauer,S. Grämlich,U. Zeimer,Ingrid Rechenberg,M. Weyers
出处
期刊:Routledge eBooks
[Routledge]
日期:2017-11-22
卷期号:: 397-400
标识
DOI:10.1201/9781315140810-81
摘要
Low temperature photoluminescence spectra of strained In x Ga 1-x As/GaAs quantum wells grown by metalorganic vapour phase epitaxy at 700° C reveal significantly higher PL line widths on substrates with 2° off-orientation than on (100) just oriented ones. Additionally, the PL intensity drops earlier when the In-supply is increased. X-ray diffraction measurements show that the higher PL line widths are related to In carry-over from the QW to the following GaAs cap. Segregation is stronger for the off-oriented InGaAs QWs leading to lower In concentration X S in the QW. These differences vanish at higher In concentrations (X S > 0.2). For high In supply (X V > 0.3) In segregation leads to the formation of dark spot defects visible in cathodoluminescence which cause a drastic decrease of the PL intensity and increase of the PL peak width. The stronger segregation effect on off-oriented substrates leads to the earlier formation of an In-rich wetting layer at the surface, as a precondition for the defect formation. So the critical layer thickness for the defect formation on the off-oriented samples is smaller than for the just oriented ones. The reduced segregation on just oriented GaAs makes the (100) orientation the preferred one for the growth of lasers with emission wavelengths above 1000 nm that require a high total In content in the InGaAs QWs.
科研通智能强力驱动
Strongly Powered by AbleSci AI