材料科学
热电效应
空位缺陷
工作(物理)
热电材料
相(物质)
热电发电机
纳米技术
光电子学
冶金
凝聚态物理
固溶体
科技与社会
工程物理
立方晶系
作者
Yuan Ye,Binrong Huang,Yugeng Li,Tu Lyu,Yitao Lu,Moran Wang,Xinjian Li,Hua‐Lu Zhuang,Chaohua Zhang,Fusheng Liu,Lipeng Hu
标识
DOI:10.1021/acsami.6c03375
摘要
Strong covalent bonding and low crystal symmetry intrinsically constrain the thermoelectric performance of orthorhombic GeSe. Here, we introduce a synergistic approach combining metavalent alloying and vacancy engineering to stabilize a high-symmetry cubic phase and activate the latent thermoelectric potential of GeSe. Incorporation of a small amount of nonstoichiometric Bi2Te3 (10%) induces a structural transition from covalently bonded orthorhombic GeSe to a metavalently bonded cubic counterpart. However, the large atomic size mismatch between Bi and Ge restricts the Bi2Te3 solubility, causing Bi2Se2Te impurity precipitation and a detrimental cubic-to-hexagonal phase transition at elevated temperatures. This high-temperature structural instability is effectively suppressed by trace Cd doping, which promotes impurity redissolution and stabilizes the cubic phase across the entire temperature range. Relative to the pristine orthorhombic phase, the stabilized cubic GeSe exhibits a narrowed bandgap, sharpened band edges, enhanced band degeneracy, softened chemical bonding, increased lattice anharmonicity, and hierarchical defect structures, collectively enabling collaborative optimization of electrical and thermal transport. Consequently, (Ge0.95Cd0.05Se)0.9(Bi2Te3)0.1 delivers a peak zT of 0.64 at 723 K, a 13-fold enhancement over pristine GeSe. This work identifies metavalent alloying coupled with vacancy engineering as an effective and general pathway for stabilizing high-symmetry cubic phase and enhancing thermoelectric performance in low-symmetry chalcogenides.
科研通智能强力驱动
Strongly Powered by AbleSci AI