法拉第效率
阳极
材料科学
阴极
化学工程
催化作用
重量分析
功率密度
溶解
电极
电解质
氧化物
电流密度
密度泛函理论
聚丙烯酸钠
碳纤维
钠
纳米技术
作者
Chunwei Li,Peiyu Zhao,Ahu Shao,Tongshuai Wang,Jiawen Tang,Wenzhuo Tan,Jiacheng Liu,Yisheng Hu,Peiwen Fan,Junyu Zhang,Yue Ma
出处
期刊:ACS Nano
[American Chemical Society]
日期:2026-11-19
标识
DOI:10.1021/acsnano.6c14733
摘要
The pursuit of higher energy and power densities in sodium-ion batteries (SIBs) is constrained by the trade-off between multielectron faradaic reaction kinetics and interfacial stability. Here, we develop a catalyst-mediated presodiation and interfacial rejuvenation strategy to address the low initial Coulombic efficiency of hard carbon (HC) anodes and transition-metal (TM) dissolution from high-voltage polyanionic and layered oxide cathodes in ampere-hour-scale pouch cells. Moving beyond empirical catalyst selection, we establish a rational screening framework for transition-metal single-atom sites based on electronic coupling and geometric compatibility with Na2S. Atomically dispersed Co (SA-Co) emerges as the preferred catalyst, reducing the Na2S decomposition potential to 3.49 V. An SA-Co/Na2S@C functional layer enables precise sodium-inventory compensation and simultaneous interfacial rejuvenation. Unlike conventional blended additives, sulfur-derived polysulfides suppress TM crossover and support high-voltage operation up to 4.5 V, while replenished sodium compensates irreversible HC losses and stabilizes the solid-electrolyte interphase. Coupling an SA-Co/Na2S@C-coated Na3V2(PO4)3 (NVP) cathode (18 mg cm–2) with an HC anode under lean-sodium and lean-electrolyte conditions (N/P ratio = 0.4; E/C ratio = 1.2 g Ah1–) yields a 1.1 Ah pouch cell retaining 97.2% capacity after 200 cycles, with gravimetric and volumetric energy densities of 317 Wh kg–1 and 485 Wh L–1, respectively, and a maximum power density of 831 W kg–1. Compatible with existing electrode manufacturing, this scalable interfacial approach offers a practical pathway toward high-energy, high-power SIBs.
科研通智能强力驱动
Strongly Powered by AbleSci AI