摘要
Linear polarisation resistance(LPR) was used to trace the corrosion rate of 3Cr pipe line steel during corrosion process.EIS and SEM were used to detect the structure of protective CO_2 corrosion product films.The appearance and evolvement of the loose internal-layer with lower Cr/Fe ration which was observed by SEM,was analyzed by EIS.Amorphous corrosion product film grew from outside to inside with time.The increase of the Cr/Fe ratio and the thickness of the film cause the decrease of momentary corrosion rate.The chromic compound produced by a certainty Cr~(3+) concentration.When the pitting corrosion suppressed,high corrosion rate in the pit resulted in high Cr~(3+) concentration which would produce much chromic compound,and in this way,the development of the pit would be prevented.
科研通智能强力驱动
Strongly Powered by AbleSci AI