Objective To obtain the optimal parameters during the electrodepositing of Ni-Cr foam alloy. Methods The main factors including the thickness,deposition rate and chrome content of the coating layer were explored by orthogonal design experiment. The coating indices for cross-section microstructure and surface morphologies were investigated by the test methods. Results A 24. 09 μm thick layer of uniform and bright coating was obtained with 14. 76 wt% of Cr at the deposition rate of 0. 4198 mg /( cm2·min) in the solution of 125 g/L CrCl3·6H2O with a pH of 2. 0 and current density of 28 A / dm2at 25 ℃ for sixty minutes. Conclusion Temperature was the most important factor affecting the Ni-Cr alloy layer thickness and deposition rate in the range of 25 ~ 40 ℃,and the concentration of CrCl3·6H2O and complexant in plating solution were the most important factors affecting the chrome content of the coating layer.