A nickel layer on the surface of polyurethane foam was prepared by electroless plating and electro-deposition process.The main factors affecting the thickness and quality of the layer such as pH value,temperature,current density were explored.Optical microscopy,scanning electron microscope and energy dispersive spectrometer were used to observe the surface morphologies,cross-section microstructure and composition of electroplated nickel layer.Experiment results show that the thickest coating obtained at pH = 4.2 is 76 μm.The coating thickness increases with increasing current density with scorched coating appeared when the current density is 11.8 A/dm2,and the optimal current density is 9.6 A/dm2.The temperature to obtain the thickest coating is 60℃ with a coating of 95 μm.Deposition thickness increases with deposit time increase.In the optimized deposition conditions,a bright,uniform and flawless nickel coating can be obtained.