材料科学
艾氏冲击强度试验
复合材料
共聚物
抗冲击性
形态学(生物学)
延展性(地球科学)
天然橡胶
聚合
聚合物
相(物质)
韧性
增韧
甲基丙烯酸甲酯
聚合物混合物
基质(化学分析)
延伸率
化学工程
作者
Xuzhao Wang,Penghao Zhang,Xinhao Guo,Baijun Liu
摘要
To address the trade‐off between transparency and impact resistance in toughened methyl methacrylate‐styrene (MS) resin and the limitations associated with emulsion‐derived MBS, transparent methyl methacrylate‐butadiene‐styrene (MBS) resin was prepared via free‐radical bulk polymerization using styrene‐butadiene‐styrene (SBS) block copolymer as the rubber phase. The effects of MMA content on SBS‐matrix interactions, rubber‐phase morphology, and macroscopic properties were systematically investigated using DMA, SEM, and DLS. At low MMA contents, stronger SBS‐matrix interactions favor the formation of small and finely dispersed rubber domains, which limits effective toughening. At 45 wt% MMA, a moderate degree of phase separation produces a favorable rubber‐domain morphology, achieving 91.2% transmittance, 3.03% haze, and a notched Izod impact strength of 7.5 kJ/m 2 . An MMA content of approximately 50 wt% represents a critical transition composition, above which pronounced SBS aggregation and rapid rubber‐domain growth occur, resulting in a marked loss of optical transparency. Increasing MMA content enhances impact resistance and matrix rigidity but reduces ductility and melt flowability. These results demonstrate that controlling matrix composition and phase morphology provides an effective strategy for balancing transparency, toughness, and processability in bulk‐polymerized MBS resins.
科研通智能强力驱动
Strongly Powered by AbleSci AI