摘要
Through glass via (TGV) technology has become a core interconnection solution for advanced electronic packaging, especially for 2.5D/3D heterogeneous integration and chiplet modules. Currently, the mainstream industrial TGV metallization adopts solid copper (Cu) electroplating filling with a thin titanium (Ti) adhesion layer. This scheme effectively improves the interfacial bonding strength between Cu conductor and glass substrate, but fails to address the thermo-mechanical coupling stress induced by the significant coefficient of thermal expansion (CTE) mismatch between Cu (CTE ~17 ppm/K) and glass (CTE ~3-5 ppm/K). Such thermal mismatch stress tends to induce glass cracking failure during thermal cycling and high-temperature service, restricting the long-term reliability of TGV devices. This paper proposes a buffer layer strategy to solve the above pain points, aiming to balance thermal stress mitigation and interfacial adhesion. The design mechanism of the ideal buffer layer is analyzed in depth, and the core selection principles of low Young's modulus, suitable ductility, and gradient CTE matching between Cu and glass are defined. For a TGV deep-hole structure with a hole depth of 450 μm, a hole diameter of 62 μm, and an aspect ratio (AR) of 7.2, four buffer layer fabrication processes—Spray Coating, Plasma-Assisted Electrospray, Spin-Coating, and Plasma-Enhanced Chemical Vapor Deposition (PECVD) —are investigated, and the polyimide (PI) organic buffer layer is ultimately identified as the optimal solution. The core mechanical performance parameters preferred for PI material are as follows: a tensile strength of 135 ± 8 MPa, an elongation at break of 45 ± 3%, and a Young's modulus of 4.2 ± 0.3 GPa, enabling efficient mitigation of thermal stress. In contrast, inorganic buffer layers (e.g., SiO2/Si3N4via PECVD) exhibit extremely limited stress buffering effect due to their high intrinsic Young's modulus. Combined with standardized reliability tests including thermal shock (-55°C to 150°C, 350 cycles) and Precon 169h damp heat aging (85°C/85% RH), the typical glass crack failure morphology of the conventional TGV-Cu structure is clearly presented. The results demonstrate that the PI buffer layer effectively suppresses crack initiation and propagation, and significantly improves the thermal reliability of TGV metallization. This research confirms the application potential of organic buffer layers in TGV reliability optimization, providing a feasible direction for the industrial development of TGV technology.