A cerium dioxide (CeO2) film with characteristic cubic lattice and optical band gap energy has been deposited chemically onto a non-conductive glass substrate at 333 K by simple immersion into an aqueous solution containing hydrous cerium(III) nitrate and dimethylamineborane (DMAB).