A new technology for preparation of sodium fluoride from silicofluoric acid was tested for comprehensive utilization of silicofluoric acid, a byproduct from phosphate fertilizer plant. First, silicofluoric acid reacted with ammonium bicarbonate at an initial n( NH4HCO3)/n( H2SiF6) ratio of 6.2-6.4 and at 35-40 ℃ for 1.0-1. 5 h and then at 75-85 ℃ for 1. 0-1. 2 h, resulting in ammonium fluoride solution with silicon dioxide sediment. Sulphuric acid was added to acidify solution for 0. 5-1. 0 h with final pH value of 6. 0-6. 5. The acidified solution was digested at 60-65 ℃ for 0. 5-1. 0 h and separated from silicon dioxide. Second, ammonium fluoride solution reacted with sodium chloride at an initial n( NH4F)/n( NaCl) ratio of 1. 0 and at 70-80 ℃ for 1. 0-1. 5 h, to form a solution containing sodium fluoride crystal and ammonium chloride. Then the solution was digested at 60-70 ℃ for 0. 5-1. 5 h and separated from ammonium chloride, leading to sodium fluoride slurry. Sodium fluoride product was collected through scrubbing and drying of the slurry. The test results showed that the quality of sodium fluoride , silica white and ammonium chloride prepared by the new technology was up to the national standard, resulting in good economic benefits.