发光
持续发光
材料科学
矿物学
化学
光电子学
热释光
作者
Bartosz Bondzior,Dagmara Stefańska,Thi Hong Quan Vu,Natalia Miniajluk-Gaweł,P.J. Dereń
标识
DOI:10.1016/j.jallcom.2020.157074
摘要
Abstract La2MgTiO6 (LMT) doped with Eu3+ ions has been prepared for the first time by the co-precipitation method. All samples crystallize in the same orthorhombic crystal structure and the unit cell volume decreases with increasing dopant concentration. The Eu3+ luminescence can be excited either into O2− → Eu3+ Charge Transfer State (CTS) with a maximum at 320 nm or into 4f levels and exhibits the emission spectrum characteristic for Eu3+ ions at the low symmetry site. TiO6 groups are also optically active with absorption at 305 nm and a weak broadband emission at 478 nm. The configurational coordinate diagram was constructed based on the absorption, emission and thermal quenching energy values. The relative thermal sensitivity of the intensity ratio between luminescence excited at 532 nm and 266 nm is above 1% for temperatures below 230 K and 3% for 77 K. The rise time of the 5D0 luminescence after the pulse excitation of the 5D1, resulting from both the multiphonon relaxation and the cross-relaxation, strongly depends on the Eu3+ concentration and goes from 94.1 μs for 0.1% Eu3+ down to 39.6 μs for 7% Eu3+. It is only observed when the sample is excited at 532 nm (into the 5D1 level). When the sample is excited into the CTS, the rise time is not observed.
科研通智能强力驱动
Strongly Powered by AbleSci AI