Abstract Carbon dioxide (CO2) stream, captured from industrial plants, usually contains impurities, such as water, oxygen, SO2, NO2 and/or H2S etc., which could lead to the exacerbated corrosion of the inside surface of supercritical CO2 transportation pipelines. Literature review shows that available corrosion database is quite limited and somewhat controversial. Our preliminary studies suggest that the existence of water and oxygen in supercritical CO2 can promote steel corrosion. In this paper, the influence of water, oxygen, the grades of CO2 sources and fluid flow rate on the corrosion performance of X42, X60, X80 and X100 steels were investigated using a rotating cage in an autoclave. The results show that steel chemistry, flow rate and the grades of CO2 sources do not have any remarkable effects on the steel corrosion. Impurity water, dissolved in supercritical CO2, only has marginal influence on the steel corrosion. The influence of oxygen on the steel corrosion is related to dissolved water content and CO2 pressure. Addition of oxygen into a pure supercritical CO2 stream does not enhance the steel corrosion. In water-saturated CO2 stream, the influence of oxygen is coherently related to the stream pressure. There is a threshold pressure value (~ 10 MPa) of the CO2 stream containing oxygen and water, above which the corrosion of pipeline steels cannot be ignored.