The thickness dependences of the crystallinity and ferroelectricity for (Al0.9Sc0.1)N films were investigated. The (001) out-of-plane orientation and ferroelectricity of (Al0.9Sc0.1)N film depend on the thickness of (Al0.9Sc0.1)N film and Pt bottom electrode. 30-nm-thick (Al0.9Sc0.1)N films deposited on 5-nm-thick Pt bottom electrodes maintain the (001) orientation and saturated high remanent polarization (Pr) (> 100 μC/cm2). We succeeded in reducing the total thickness of the Pt bottom electrode and (Al0.9Sc0.1)N film to 35 nm.