作者
Anna Pražanová,Jonáš Uřičář,Zbyněk Plachý,Jiřı́ Brožek,Václav Knap,Daniel‐Ioan Stroe
摘要
The transition to all-solid-state lithium-ion batteries requires electrolytes with both high ionic conductivity and sufficient mechanical integrity to replace conventional separators and liquid electrolytes. Conventional polyethylene oxide (PEO)-based polymer electrolytes typically exhibit room-temperature ionic conductivities on the order of 10 -7 –10 -6 S·cm -1 and crystalline fractions exceeding 60 %, which severely restrict Li + transport [1]. In addition, the tensile strength of pure PEO films commonly remains below 3 MPa, which poses risks for mechanical failure and internal short circuits during battery assembly and operation [2]. To address these limitations, a composite polymer electrolyte (CPE) concept (Fig. 1) was developed. It comprises a PEO matrix with deliberately lower molecular weight ( M W ≈ 400,000 g·mol⁻¹) containing lithium bis((trifluoromethyl)sulfonyl)amide (LiTFSI), integrated with an electrospun polyamide 4 (PA4) nanofiber scaffold. Using lower- M W PEO is expected to increase segmental mobility and expand the amorphous phase fraction by ~20–30 %, potentially raising intrinsic Li + conductivity by one to two orders of magnitude compared with high- M W PEO (≈600,000 g·mol -1 ) [3]. The PA4 scaffold offsets the reduced mechanical robustness, offering an anticipated tensile strength exceeding 9.2 MPa and a ratio of polar amide group (-CO-NH-) to -CH 2 - in repeating unit (1:3) which is approximately 30% higher than that of PA6 (1:5). This enables more efficient Li + coordination and salt dissociation [3,4]. The hierarchical PA4 architecture, consisting of intertwined micro- and nanofibers, is expected to facilitate uniform ionic flux by providing a high density of continuous adsorption sites, resulting in a more homogeneous current distribution and supporting stable lithium intercalation into the graphite anode relative to unreinforced PEO systems. Preliminary structural and thermal assessments indicate stable interfacial interactions between PA4 and PEO, suggesting favorable long-term cycling behavior. Although electrochemical measurements are ongoing, the synergistic improvements in PEO segmental dynamics and PA4 mechanical reinforcement are anticipated to enable ionic conductivities approaching 10 -4 S·cm -1 at moderate temperatures and substantially extended cycling stability in full cells utilizing a graphite anode and a LiFePO 4 (LFP) cathode [2,3]. This composite design therefore provides a mechanistically grounded pathway toward high-performance all-solid-state electrolytes for next-generation lithium-ion batteries. Acknowledgements This work was funded by the EU NextGenerationEU through the Recovery and Resilience Plan for Slovakia under the project SUNFLOWERS No. 09I02-03-V01-00022. Additionally, the infrastructure used was made available through the project “The Energy Conversion and Storage”, funded as project no. CZ.02.01.01/00/22_008/0004617 by Programme Johannes Amos Comenius, call Excellent Research. Furthermore, this work is financially supported by the Grant Agency of the CTU in Prague, grant no. SGS24/136/OHK3/3T/13. References Chattopadhyay, J.; Pathak, T.S.; Santos, D.M.F. Applications of Polymer Electrolytes in Lithium-Ion Batteries: A Review. Polym. 2023, Vol. 15, Page 3907 2023, 15 , 3907, doi:10.3390/POLYM15193907. Gao, L.; Li, J.; Ju, J.; Cheng, B.; Kang, W.; Deng, N. High-Performance All-Solid-State Polymer Electrolyte with Fast Conductivity Pathway Formed by Hierarchical Structure Polyamide 6 Nanofiber for Lithium Metal Battery. J. Energy Chem. 2021, 54 , 644–654, doi:10.1016/J.JECHEM.2020.06.035. Martin-Ortiz, J.; Blanco, J.; Armand, M.; Otaegui, L.; Morant-Miñana, M.C.; Villaverde, A. Influence of the PEO Molecular Weight on the Processability and Performance of SSB Cathode Composite Electrodes. J. Power Sources 2024, 623 , 235390, doi:10.1016/J.JPOWSOUR.2024.235390. Li, Y.; Li, Q.; Tan, Z. A Review of Electrospun Nanofiber-Based Separators for Rechargeable Lithium-Ion Batteries. J. Power Sources 2019, 443 , 227262, doi:10.1016/J.JPOWSOUR.2019.227262. Figure 1