金属间化合物
退火(玻璃)
分析化学(期刊)
铜
扩散
铝
薄膜
活化能
化学
材料科学
热力学
纳米技术
物理化学
冶金
物理
色谱法
合金
作者
H. T. G. Hentzell,K. N. Tu
摘要
Isolated W islands, 150 Å in diameter, have been deposited between Cu and Al thin film bilayers to serve as inert diffusion markers. Marker displacements have been measured consecutively by Rutherford backscattering spectroscopy during the sequential growth of CuAl2, CuAl, and Cu9Al4 intermetallic compounds upon annealing in the temperature range 160–250 °C. The intrinsic interdiffusion coefficients of Al and Cu in each of these compounds have been determined by applying an analysis of marker motion in a binary diffusion couple to the measured displacement data. Moreover, the prefactor and activation energy of the individual diffusivities have been calculated as shown below by measuring the marker motion as a function of temperature. For CuAl2, D0Al =0.4 cm2/s, QAl =1.25±0.05 eV, D0Cu =9.5 cm2/s, QCu =1.40±0.05 eV. For CuAl, D0Al =1.5×10−7 cm2/s, QAl =0.7±0.05 eV, D0Cu =1×10−2 cm2/s, QCu =1.1±0.05 eV. For Cu9Al4, D0Al =1.7×10−3 cm2/s, QAl =1.20±0.05 eV, D0Cu =2.4×10−2 cm2/s, QCu =1.30±0.05 eV. These values agree quite well to those chemical interdiffusion coefficients published in the literature for bulk samples. A discussion on sequential compound formation has been given on the basis of these measured values.
科研通智能强力驱动
Strongly Powered by AbleSci AI