摘要
This study examined the effects of localized degradation and Ni–Co coating in a large-area solid oxide fuel cell (SOFC) operated under hydrogen and direct ammonia fueling. Comparable electrochemical performances were achieved under both conditions, with the exception of the power density loss caused by the high contact resistance in the test configuration. Complete ammonia conversion occurred at 650 °C under a low normalized flow rate with a large active area, emphasizing the importance of the residence time. Post-test analyses revealed pronounced degradation in the inlet region of the anode and the current collector, where repeated nitridation/reduction cycles led to Ni particle coarsening, microstructural collapse, and weakening of the current pathways. In contrast, the outlet region exhibited minimal structural changes, confirming that degradation was highly site-specific. Ammonia exposure tests performed on ferritic stainless-steel interconnectors demonstrated that the Ni–Co coating suppressed nitride formation and preserved the structural integrity, mitigating nitrogen ingress. These results indicate that the durability challenges associated with direct-ammonia SOFCs are governed by localized inlet-side degradation. Region-specific protection of the anode and current collector, together with Ni–Co coating, are proposed as practical strategies to improve the long-term stabilities and reliabilities of SOFC stacks under direct ammonia operation.
科研通智能强力驱动
Strongly Powered by AbleSci AI