材料科学
烧结
扫描电子显微镜
碳化硅
相(物质)
衍射
碳化物
碳化钛
摩尔比
化学工程
分析化学(期刊)
复合材料
光学
工程类
催化作用
有机化学
化学
物理
生物化学
色谱法
作者
Songlan Yang,ZhengMing Sun,Hitoshi Hashimoto
标识
DOI:10.1007/s10019-003-0255-1
摘要
Ti/Si/TiC powder mixture with molar ratios of 2: 2: 3 were sintered at various temperatures from 700–1300 °C for 15 min by PDS technique. X-ray diffraction (XRD) and scanning electron microscopy (SEM) were used for the evaluation of phase composition in different samples for the understanding of the sintering mechanism for this system. Results showed that Ti5Si3 formed as the intermediate phase during sintering. The reaction between Ti5Si3 and TiC as well as Si induces the formation of Ti3SiC2, and TiSi2 appears as the byproduct in this process. At temperature above 1000 °C, TiSi2 reacts with TiC to form Ti3SiC2. High Ti3SiC2 phase content bulk material can be synthesized at 1300 °C for 15 min.