Low-Temperature Solid-State Synthesis of Zirconium Dioxide via Thermal Decomposition of ZrOCl2·8H2O–NaHCO3 Mixtures: Kinetics, Morphological Control by In Situ NaCl Matrix, and Comparison with Established Crystalline ZrO2 Phases
作者
Володимир Трихліб
出处
期刊:日期:2026-06-23
标识
DOI:10.26434/chemrxiv.15005082/v1
摘要
The thermal decomposition of a solid-state mixture of zirconyl chloride octahydrate (ZrOCl2·8H2O) and sodium bicarbonate (NaHCO3) was investigated by simultaneous thermogravimetry / differential thermogravimetry / differential thermal analysis (TG/DTG/DTA) over the temperature range 90–250 °C. A pronounced synergistic effect was identified: the maximum mass-loss rate (DTG minimum) of the mixture occurs at 120.0 °C—some 35 °C below that of pure NaHCO3 (155.1 °C) and 15 °C below that of pure ZrOCl2·8H2O (135.1 °C)—while the endothermic DTA peak is dramatically attenuated (−14.9 mV vs. −120.1 mV for the pure oxychloride). Activation energies determined by the Friedman isoconversional method are ≈41 kJ mol-1 (mixture), ≈68 kJ mol-1 (NaHCO3), and ≈110 kJ mol-1 (ZrOCl2·8H2O). The low activation energy is attributed to in situ HCl neutralisation by NaHCO3, which prevents back-reaction and drives the equilibrium towards ZrO2. Crucially, NaCl—co-formed in equimolar quantity with ZrO2—acts as a solid-state spacer matrix that suppresses particle sintering and promotes anisotropic, platelet-like ZrO2 morphology, in sharp contrast to the spherical/polygonal particles obtained by high-temperature routes (>800 °C) described in literature [1–3]. The product is characterised against CAS 1314-23-4 and ASTM C1065 reference data. These results provide a low-energy, aqueous-waste-free pathway to nanostructured ZrO2 with controllable morphology relevant to ceramics, catalysis, and nuclear-grade oxide applications.