The Cu-Sn-P alloy coating on the surface of A3 steel was prepared by the technology of electroless plating in the new formula conditions.The influence of the bath composition and deposition condition on the coating was discussed.The Cu-Sn-P/stearic acid(lauric acid,BTA)electroless coatings were prepared by treating the alloy coating of the Cu-Sn-P with BTA (benzeneazimide),stearic acid and lauric acid respectively,and the protecting complex film with density was then made.The properties of Cu-Sn-P/stearic acid(lauric acid,BTA)electroless coatings were also investigated.