脱质子化
材料科学
芳纶
剥脱关节
纳米纤维
膜
纳米尺度
延展性(地球科学)
极限抗拉强度
纳米技术
质子
化学工程
动力学
拉伸试验
工作(物理)
复合材料
高分子
作者
Weiwei Li,Jinxue Lei,Hongli Mi,Ting Chen,Xuan Li,Meiyun Zhang
标识
DOI:10.1021/acsami.6c16767
摘要
Aramid nanofibers (ANFs) are promising high-performance nanoscale building blocks, yet their application is hindered by the time-consuming conventional deprotonation method. This study systematically compares this traditional method with a proton donor-coupled deprotonation (PCD) strategy. While both preserve the core chemical structure of PPTA fibers, the PCD approach, by incorporating a proton donor, dramatically alters the reaction kinetics and nanofibrillation pathway. Comprehensive characterization confirms that it accelerates exfoliation from days to 4 h, yielding a highly transparent dispersion. Crucially, the synthesis pathway dictates the final nanomorphology: conventional ANFs form rigid networks with larger pores (∼44 nm), whereas PCD-derived ANFs are more interconnected and pliable, self-assembling into denser membranes with finer pores (∼9 nm). This structural divergence translates to superior integrated mechanical performance, with PCD-ANF membranes exhibiting a remarkable balance of high tensile strength (115.14 MPa) and good ductility (19.27%), alongside fully retained inherent flame retardancy. This work establishes fundamental structureproperty relationships, demonstrating that the choice of nanofibrillation mechanism is a powerful tool for tailoring nanoscale architecture in advanced functional materials.
科研通智能强力驱动
Strongly Powered by AbleSci AI