Yongkang Ma,Zhiwei Zhao,Yan Wang,Ziqiang Qiao,Hongjuan Zheng
标识
DOI:10.1016/j.jmrt.2026.08.208
摘要
Combining smaller and larger WC grain populations within a single cemented-carbide matrix offers a microstructural route for mitigating the conventional hardness–toughness trade-off. Nevertheless, retaining this heterogeneous grain-size architecture during SPS remains challenging because of non-uniform WC grain evolution, discontinuous binder distribution, and local interfacial heterogeneity. This work integrates a sequentially optimized Cr 3 C 2 –Y 2 O 3 /La 2 O 3 interfacial-regulation strategy with an SPS-processed dual-scale WC–Co–Ni matrix. The additive contents and SPS parameters were optimized sequentially, and the resulting phase constitution, grain-size evolution, near-surface chemical states, and local interfacial structures were evaluated using complementary XRD, XPS, EBSD, and TEM analyses. The optimized sample, containing 0.6 wt.% Cr 3 C 2 and 0.10 wt.% total Y 2 O 3 /La 2 O 3 at a Y 2 O 3 :La 2 O 3 mass ratio of 1:1 and sintered at 1400 °C for 6 min under 40 MPa, achieved a hardness of 2036.43 HV30 and an indentation fracture toughness of 13.12 MPa·m 1/2 . Microscopy and elemental mapping indicated Cr-containing carbide-related interfacial transition regions and localized Y–La–O-bearing regions near grain boundaries and triple junctions. The pure fine-grained sample exhibited the lowest apparent initial-stage oxidation rate constant, whereas the optimized composite-inhibitor sample showed a lower value than the optimized dual-scale control. The COF curves and worn-surface observations characterize the sliding response. Therefore, the principal demonstrated advantage of the optimized composite-inhibitor sample is its hardness–toughness balance, while the oxidation and sliding results highlight areas requiring further optimization.
科研通智能强力驱动
Strongly Powered by AbleSci AI