材料科学
放电等离子烧结
光催化
正交晶系
三氧化钨
钨
魔角纺纱
烧结
分析化学(期刊)
结晶学
催化作用
晶体结构
核磁共振
冶金
核磁共振波谱
物理
化学
生物化学
色谱法
作者
Martin Lange,Yaşar Krysiak,Jens Hartmann,Georg F. Dewald,Giacomo Cerretti,Muhammad Nawaz Tahir,Martin Panthöfer,Bastian Barton,Tobias Reich,Wolfgang G. Zeier,Mihail Mondeshki,Ute Kolb,Wolfgang Tremel
标识
DOI:10.1002/adfm.201909051
摘要
Solid state reactions are notoriously slow, because the rate‐limiting step is diffusion of atoms or ions through reactant, intermediate, and product crystalline phases. This requires days or even weeks of high temperature treatment, consuming large amounts of energy. Metal oxides are particularly difficult to react, because they have high melting points. The study reports a high‐speed solid state fluorination of WO3 with Teflon to the oxyfluorides WO3–xFx on a minute (<10 min) scale by spark plasma sintering, a technique that is used typically for a high‐speed consolidation of powders. Automated electron diffraction analysis reveals an orthorhombic ReO3‐type structure of WO3–xFx with F atom disorder as demonstrated by 19F magic angle spinning nuclear magnetic resonance spectroscopy. The potential of this new approach is demonstrated by the following results. i) Mixed‐ valent tungsten oxide fluorides WO3–xFx with high F content (0 < x < 0.65) are obtained as metastable products in copious amounts within minutes. ii) The spark plasma sintering technique yields WO3–xFx nanoparticles with high photocatalytic activity, whereas the corresponding bulk phases obtained by conventional solid‐state (ampoule) reactions have no photocatalytic activity. iii) The catalytic activity is caused by the microstructure originating from the processing by spark plasma sintering.
科研通智能强力驱动
Strongly Powered by AbleSci AI