溶剂化
锌
化学
电池(电)
金属
熵(时间箭头)
计算化学
无机化学
热力学
有机化学
物理
分子
功率(物理)
作者
Kangning Zhao,Linhui Chang,Hongwei Cheng,Jiamin Li,Lei Zhang,Bomian Zhang,Lihen Zheng,Qiangchao Sun,Jiantao Li,Xionggang Lu
标识
DOI:10.21203/rs.3.rs-4870452/v1
摘要
Abstract Aqueous zinc-ion batteries offer sustainable large-scale storage potential with inherent safety and low cost, yet suffer from limited energy density and cycle life due to aqueous electrolyte constraints. Here, we introduce affordable, stable electrolyte (0.33 $·kg−1) incorporating minimal multi-halogen anions (Cl-, Br-, and I-) to create a high-entropy solvation structure enabling high-performance zinc batteries. Despite the small amount, the diversified mono-halogenated contact ion pair and multi-halogenated aggregate solvation structures create the unique high-entropy solvation structure, to form the lean water halogenated interfacial environment, suppressing the hydrogen evolution reaction, while facilitating cascade desolvation. Multi-halogen additives generate diverse contact ion pairs (Zn-X, X=Cl/Br/I) with compact solvation shells accelerating ion transport. In this way, the high-entropy solvation structure breaks the trade-off between plating overpotential (energy efficiency) and plating/stripping reversibility (Coulombic efficiency). As a result, the high-entropy solvation-based electrolyte enables practical zinc metal battery with 152.2 Wh kg-1electrode for 120 cycles at lean electrolyte of 2.4 μL mg-1 and an Ah-level pouch cell is validated with high Coulombic efficiency of over 99.90% for over 250 cycles. Our findings emphasize the importance of electrolyte design for the precise control of anion-cation interactions for stable Zn/electrolyte interface and enable practical zinc metal battery with high energy and low cost.
科研通智能强力驱动
Strongly Powered by AbleSci AI