旋节分解
材料科学
无定形固体
亚稳态
旋节
微观结构
成核
相图
结晶
相(物质)
电介质
退火(玻璃)
硅酸盐
化学工程
化学物理
热力学
结晶学
化学
冶金
有机化学
光电子学
物理
工程类
作者
Susanne Stemmer,Zhiqiang Chen,Carlos G. Levi,Patrick S. Lysaght,Brendan J. Foran,John A. Gisby,Jeff R. Taylor
摘要
Using the concept of metastable phase diagrams, we discuss the microstructure evolution during annealing of amorphous ZrO 2 –SiO 2 and HfO 2 –SiO 2 thin films for gate dielectric applications. These systems are characterized by a low solid solubility, a liquid miscibility gap and a kinetic barrier to the formation of the complex, crystalline silicate. We show that phase partitioning is expected for most compositions. Compositions within the metastable extensions of the spinodal are unstable and will spontaneously unmix in the amorphous phase upon heating. Hafnia- or zirconia-rich phases will subsequently crystallize to form HfO 2 or ZrO 2 . Most compositions outside the metastable extensions of the liquid phase miscibility gap must phase separate above the crystallization temperature by nucleation of crystalline HfO 2 or ZrO 2 out of an amorphous silica-rich matrix. We present calculations of the metastable extensions of the miscibility gap and spinodal. The calculations predict that SiO 2 -rich compositions, investigated for gate dielectric applications, will show spinodal decomposition if they contain less than ∼90 mol% SiO 2 at the typical device processing temperature of 1000°C. Experimental studies of Hf-silicate films with three different compositions, between ∼40 and 80 mol% HfO 2 that lie inside and outside the miscibility gap, respectively, are presented. All three compositions show phase separation. Despite the different pathways of microstructure evolution, the final phase separated microstructures are similar. Experimental verification of the pathways that lead to these microstructures requires further studies.
科研通智能强力驱动
Strongly Powered by AbleSci AI