C S. CARTER,D.G. Farwick,Alan M Ross,Jack M. Uchida
出处
期刊:Corrosion
[NACE International]
日期:1971-05-01
卷期号:27 (5): 190-197
被引量:45
标识
DOI:10.5006/0010-9312-27.5.190
摘要
The plane-strain fracture toughness KIc and stress corrosion threshold KIscc (in 3.5% aqueous sodium chloride solution) have been determined for the following high strength, precipitation hardening steels: 17-7 PH (RH 950, TH 1050), PH 15-7Mo (RH 950, TH 1050), AM 355 (SCT 850, SCT 1000), AM 362 (H 900, H 1000), AM 364 (H 850, H 950), 17-4 PH (H 900, H 1000), 15-5 PH air melted and vacuum melted (H 900, H 1000), PH 13-8Mo (H 950), and Custom 455 (H 950). Correlations of KIscc with service performance and smooth-specimen test data are discussed.