Introduction It is common practice in the petroleum industry to apply two ASTM standard corrosion tests (o corrosion resistant alloys (CRAs) as a means to determine their relative corrosion resistance compared to other alloys and as a quality control method to ensure no manufacturing processes have promised this corrosion resistance. The ASTM G 48 test for pitting resistance in ferric chloride solution is applied in both cases above and the ASTM A 262 Practice E is used in the latter. The A 262 Practice E is also required by API 5LD. Although the G 48 test has generally been successfully applied for ranking the pitting resistance of stainless steel and some nickel base alloys the application of the G 48 and A 262 tests for manufacturing control and for the evaluation of welding procedures has been less than satisfactory, often leadingto conflicting results. This paper will not attempt to explore all of the myriad problems that have been encountered in applying these two tests but instead on two speed problems that are consistently encountered in evaluating the welding of CRA lined and clad Iine pipe. These two problems are the testing of the inside surface of the liner and red pass of a girth weld to determine the effect of discolouration (heat tint) on the corrosion resistance of the weldment and selective corrosion of the test coupon from the backside (i.e. the side of the cladding or liner on the side nearest the steel) of the test coupon in preference to the root bead side. In both cases the tests are carried out using the G 48 Method A, generally at 22-25° C for 72 hours. Standard Test Method and Variations The standard G 48 and A 262 tests specific that the test specimens be polished to a uniform finish on all surfaces with a 120-grit abrasive paper. Figure 1 shows how manufacturers and test laboratories often prepare the test coupon. It is obvious that this means of coupon preparation will not test the actual surface properties of the material tier fabrication and furthermore, it is doubtful that the pitting behavior will be affected at all for a coupon of this type regardless of the condition of the inside surface of the clad or liner weldment. Yet it is in keeping with the requirements for coupon preparation according to A 262 and G 48. For clad and lined pipe welds it is imperative that the back side of the coupon representing the side facing the steel be thoroughly machined to remove iron contaminants that can compromise the test results by producing premature pitting and corrosion on that side before pitting can proceed on the root side of the coupon. It is more appropriate to leave the root bead and CRA clad or liner inside surface in its original condition in order to determine the behavior of these weldments in service.